2 rotor grafit komposit, kontrol kecepatan frekuensi variabel 0‑600rpm
Throughput aluminium cair:
25‑35 ton/jam
Hidrogen saluran keluar (Saluran masuk<0,28mL/100g):
≤0,12 mL/100g
Persyaratan gas inert:
Kemurnian≥99,996%, titik embun<‑69℃
Akurasi kontrol suhu:
±2 ℃
Hidrogen keluar (saluran masuk>0,28mL/100g):
≤0,14 mL/100g
Menyediakan kemampuan:
600 buah/tahun
Menyoroti:
in-line degassing unit for aluminum melting
,
continuous casting machine degassing parts
,
blowhole defect reduction casting retrofit
Deskripsi Produk
A compact, retrofittable in-line degassing solution engineered for continuous aluminum billet casting lines — suppressing blowhole defects and improving melt quality within limited installation space. Blowhole Control Challenges in Aluminum Billet Line Retrofit When aluminum mills upgrade older production lines, the original launder systems typically lack in-line melt purification units. After refining in holding furnaces, molten aluminum continuously reabsorbs hydrogen while